Two Component, Low Viscosity Room Temperature Curable, Epoxy Adhesive, Sealant, Coating & Casting System Featuring Both Outstanding Chemical Resistance is NASA low outgassing approved.
One component, heat cured epoxy system for bonding, sealing, dam-and-fill applications. Resists temperatures up to +600°F. Thermally conductive, electrically insulating.
Two Component, Room Temperature Curable Epoxy Adhesive, Sealant, Coating and Encapsulating System, Featuring Outstanding Chemical Resistance to Solvents, Alcohols and Fuels.
Two Component, Room Temperature Curable Epoxy Adhesive, Sealant, Coating and Encapsulating System, Featuring Outstanding Chemical Resistance to Solvents, Alcohols and Fuels.