The glass transition temperature for a given compound is reported as a single temperature, Tg, which represents the range of temperatures over which a cured epoxy transitions from a glassy, hard state to a more rubbery, softer state.
High glass transition epoxy compounds are of paramount importance to the selection of adhesives/sealants for elevated temperature applications. These products exhibit superior mechanical, thermal and electrical properties than lower Tg materials at high temperatures. Master Bond offers a versatile selection of high Tg materials to meet specific application requirements.
Certifications for High Tg Epoxies
Specific Master Bond one and two part systems meet the following certifications:
- USP Class VI for biocompatibility
- NASA low outgassing
- RoHS
- Halogen free
Learn more about the importance of Tg in selecting the right epoxy.
Most Popular Products with High Glass Transition Temperature
![]() |
UV25 Multi-purpose, one part UV curing system for bonding, sealing, coating and encapsulation. Excellent optical clarity, superb physical properties, moderate viscosity. Ultra high glass transition temperature (Tg) over 180°C. Fast fixture times. Rapid curing. Serviceable from -60°F to +500°F. |
![]() |
EP17HT Serviceable up to 600°F. Exceptional Tg of 220-225°C. No mix formulation. Low exotherm upon curing. Exemplary chemical resistance. Can be used in encapsulations and castings beyond 1/2 inch thickness. |
![]() |
EP65HT-1 Two part, fast setting (3-5 minutes in 10-20 gram masses) room temperature curing epoxy. Serviceable from -60°F to +400°F. Tg of 125-130C. NASA low outgassing approved. Used by Boeing in various MRO applications. High tensile modulus. Excellent dimensional stability. Withstands 1,000 hours 85°C/85%RH. Can be applied with gun dispenser. |
![]() |
Supreme 10HT One part structural epoxy with high bond strength and excellent adhesion to similar and dissimilar substrates, especially composite materials. Requires oven curing at 250-300°F. NASA low outgassing approved. Serviceable from 4k to +400°F. Tough and durable. 85°C/85% RH resistance. |
![]() |
EP126TK Two part toughened epoxy system. Capable of continuous service at 600°F. 100% reactive. Unmatched durability. Outstanding chemical resistance. Robust physical strength profile. Dimensionally stable. Machineable. Withstands rigorous thermal cycling. Service operating temperature range from -80°F to +600°F. |
![]() |
EP62-1 Cures rapidly at moderate elevated temperatures. Superior resistance to moisture. Two part epoxy has long pot life at ambient temperatures. High bond strength properties. Reliable electrical insulator. Serviceable from -60°F to +450°F. Withstands aggressive chemical exposure. Tg 160-165°C. Shore D hardnes >80. |
![]() |