For structural adhesives that resist exposure to water, humidity and steam, Master Bond offers a complete line of epoxies, silicones, polyurethanes, polysulfides and UV curable adhesives.
Important Performance Properties for Master Bond Water Resistant Structural Adhesives
We make specific grades of water resistant systems with enhanced performance properties, including but not limited to:
- Abrasion resistance
 - Excellent dielectric properties
 - Vibration, shock, impact and thermal cycling resistance
 - Extraordinary chemical resistance
 
Additionally, they are available for use in a range of viscosities and hardness, cure speeds and colors.
Adequate product protection is essential to prevent premature failure from moisture. Systems are engineered to maintain their physical strength properties, prevent degradation at the substrate adhesive interface, while providing effective sealing capability. These durable polymeric products have been developed to address specific needs and susceptibility to moisture attack which can cause rupturing, delamination, swelling, cracking, shrinkage, blistering. They effectively mitigate corrosion, have superior resistance to water permeation, adhere well to multiple substrates and provide long term durability after aging. These user friendly, solvent free compositions can withstand a combination of stress, moisture, temperature.
Master Bond’s Most Popular Water Resistant Systems
                        | 
                  
            EP42HT-2 Bonding, sealing, coating, potting compound. Heat, chemical, steam resistant. Superior optical transmission properties. Solvent free. Withstands exposure to acids, alkalis and many solvents. Castable up to 2-3 inches. Cures readily at ambient temperature. Service temperature range -60°F to +450°F.  | 
              
                        | 
                  
            EP3HTMed Rapid curing, one part epoxy. Meets USP Class VI biocompatibility standards. Thixotropic paste viscosity. High shear strength. Superb resistance to autoclaving, chemical sterilants, radition, EtO. Serviceable from -60°F to +400°F.  | 
              
                        | 
                  
            EP41SMed Biocompatible. Meets USP Class VI test specification. Impressive resistance to chemical sterilants including ethylene oxide, bleach, glutaraldehyde, hydrogen peroxide based systems and paracetic acid type compounds. High bond strength. Electrical insulator. Fast curing. Quick handling time. Service temperature range -60°F to +250°F.  | 
              
                        | 
                  
            EP38 Electrically insulative compound. Excellent flowability. High flexibility. Superior tensile and compressive strength. Cures quickly. Outstanding optical clarity. Protect against boiling water. Short tack free time. Low shrinkage upon cure. Easy to apply by roller, brush, spray equipment. Serviceable from -60°F to +250°F.  | 
              
                        | 
                  
            EP30NS Moderate viscosity Nanosilica epoxy resin system. High strength rigid bonds. Lower linear shrinkage after cure. Serviceable from -60°F to +300°F. Cures readily at room temperature. Passes ASTM E595 for NASA low outgassing.  | 
              
			      