Master Bond EP3HTMed medical grade epoxy was used in a patent in the field of drug delivery and pulmonary therapy, specifically, the aerosolization of liquid medicament into fine liquid droplets for inhalation.
One part, heat curing, biocompatible epoxy compound
Key Features
- One component, no mix system
 - USP Class VI certified
 - Passes ISO 10993-5 for cytotoxicity
 - Resists repeated sterilization
 
Product Description
Master Bond EP3HTMed is a one part system that combines easy processing with excellent physical strength and bonding properties. It fully meets USP Class VI specifications. It is easy to use as it does not require any mixing. It cures by heating at 250°F for 20-30 minutes, or at +300°F for 5-10 minutes. To optimize properties, use one of these cure options followed by a heat cure of 250 to 300°F for 1 to 3 hours. It should be emphasized that this is not a premixed and frozen type system. Its working life is unlimited as it will not cure until heated to the required temperature. Also, it has low shrinkage upon curing.
It bonds well to a wide variety of substrates including glass, metals, ceramics and most plastics and has superb physical strength properties. EP3HTMed also offers good electrical insulation properties. The service temperature is -60°F to +400°F. It is 100% reactive and does not contain any diluents or solvents. EP3HTMed possesses superior chemical resistance, particularly to chemical sterilants, as well as to other types of sterilization including EtO, radiation and especially autoclaving. The color of EP3HTMed is brown to tan. This medical grade epoxy is widely used in the manufacturing and production of both disposable and non-disposable devices where superior physical properties, fast curing and high performance are paramount and heat curing at 250°F is feasible.
Product Advantages
- One part, no mixing needed
 - Unlimited working life at room temperature
 - Easily applied
 - Superb resistance to autoclaving, chemical sterilants, radiation and EtO
 - Excellent adhesion to many substrates and superior physical properties
 
Featured Product: Richard Wolf Medical Instruments Corporation, Flexible Endoscope.
Industrial Certifications
Packaging
EP3HTMed is available is various sizes and units to accommodate customer's needs.
Case Studies
Master Bond EP3HTMed medical grade epoxy was used in a patent in the field of drug delivery and pulmonary therapy, specifically, the aerosolization of liquid medicament into fine liquid droplets for inhalation.
Visual Media
Master Bond EP3HTMed fully meets USP Class VI requirements and is formulated to cure rapidly at elevated temperatures. It has excellent resistance to multiple cycles of radiation, EtO, autoclaving and chemical sterilants.
			      