Special Master Bond one and two component epoxy systems offer outstanding flexural strength properties. Formulations are designed to provide high performance and excellent adhesion to similar and dissimilar substrates. Additionally, they feature superior thermal stability, exceptional chemical resistance and convenient cure schedules.
Selecting the most suitable adhesive requires careful evaluation of the bending properties under incremental loads for different specimens/thicknesses. Determination of the failure point and resisting deformation is of prime importance for structural applications under high stress conditions. This allows engineers design flexibility, light weight construction, achievable bond strength, proper preparation of difficult bonding surfaces, aging resistance and extending product longevity. High flexural strength adhesive products have been successfully employed over large bonding surfaces, for adhering substrates with dissimilar coefficients of expansion, for static/dynamic loading and for fast processing.
Popular Flexural Epoxy Compounds
                        | 
                  
            EP31 Ultra high strength, two part epoxy adhesive that bonds well to most metals and plastics. Aluminum to aluminum lap shear strength exceeds 4,000 psi. T-peel strength >50 pli. Ambient temperature curing. Tough and resilient bonds. Combines low viscosity and optical clarity. Serviceable from -60°F to +250°F. Chemical resistant. First class electrical insulator.  | 
              
                        | 
                  
            Supreme 10HT One part structural epoxy with high bond strength and excellent adhesion to similar and dissimilar substrates, especially composite materials. Requires oven curing at 250-300°F. NASA low outgassing approved. Serviceable from 4k to +400°F. Tough and durable. 85°C/85% RH resistance.  | 
              
                        | 
                  
            Supreme 45HTQ Two component, toughened, quartz filled epoxy with exceptional abrasion resistance. Heat curing system. Long working life after mixing. High compressive strength. Superb dimensional stability. Serviceable from -60°F to +450°F. Withstands exposure to petrochemicals acids, bases, solvents. Good strength retention at elevated temperatures. Successfully tested for 1,000 at 85°C/85% RH.  | 
              
                        | 
                  
            EP30LTE-4 Extra low thermal expansion coefficient and unmatched dimensional stability. Used for bonding, sealing, coating, casting. Service operating temperature range from -60°F to +250°F. Mixed viscosity 15,000-20,000 cps. Ambient temperature curing.  | 
              
			      