MasterSil 920-LO Product Information

MasterSil 920-LO One Part Silicone System

One Component, Room Temperature Curing Silicone Elastomer Adhesive
for High Performance Bonding and Sealing. Fast Curing and Non-Corrosive.
Meets MIL-A-46146.

EP46HT-1ND-2 Product Information

EP46HT-1ND2 Two Part Epoxy System

Two Component, Heat Resistant, Epoxy System for High Performance Bonding, Sealing and Casting. Features a Glass Transition Temperature in Excess of 220°C; Requires Elevated Temperature Curing at 250°F or Above.

EP46HT-2ND2 Product Information

EP46HT-2ND2 Two Part Epoxy Compound

Two Component, Heat Resistant, Epoxy System for High Performance Bonding, Sealing and Casting. Features a Glass Transition Temperature in Excess of 220°C; Requires Elevated Temperature Curing at 250°F or Above.

EP21HT-LO Product Information

EP21HT-LO Two Part Epoxy System

Two Component, Room Temperature Curing Adhesive, Sealant & Coating Featuring Convenient 1:1 Mix Ratio and High Temperature Serviceability Up To 400°F Conforms Title 21, U.S. Code of Federal Regulations, FDA Chapter 1, Section 175.105 for Food Applications

EP62-1LPSP Product Information

Two Component Epoxy System Features a Very Long Pot Life at Ambient Temperatures Combined with Rapid Cures Chemical and High Temperature Resistance

EP46CA-1 Product Information

EP46CA-1 Two Part Epoxy

Two component epoxy for structural bonding featuring superlative heat resistance; requires oven curing.

MB600SCN Product Information

MB600SCN One Part Sodium Silicate Coating

One Component Sodium Silicate, Aqueous Based Silver Conductive Coating System Featuring Awesome Shielding Effectiveness, Temperature Resistance Up To 700°F and Easy Application.

Supreme 45HTND-2 Product Information

Supreme 45HTND-2 Two Part Epoxy

Two Component, High Temperature Resistant Epoxy System for High Performance Bonding, Sealing and Coating Featuring Superior Thermal Cycling Capabilities.

EP121CL-LO Product Information

EP121CL-LO Two Part Epoxy

Two component epoxy for potting, encapsulation, coating and sealing applications