High, medium, low viscosity products will polymerize often in seconds upon exposure to a UV light source at the proper wavelength/intensity. These adhesives are not oxygen inhibited and require no heat to cure. They are ideal for bonding heat sensitive substrates. Master Bond UV cure adhesives eliminate the need for measuring, mixing, pot life issues, ovens and minimize waste. These highly reliable adhesives can be applied manually/automatically and reduce labor costs, regulatory expenses, energy/electricity while shortening cycle times. They have proven cost effective as an alternative to other joining methods.
UV adhesives are used extensively for precise positioning/alignment of parts. Compounds can be employed for structural or temporary bonding. Master Bond UV cure adhesives bond well to similar/dissimilar substrates including metals, rubbers, glass, ceramics, plastics such as polycarbonates, acrylics, phenolics. Specific grades offer optical clarity/translucency, dimensional stability, low shrinkage, resistance to chemicals, fuels, solvents, moisture. Products provide protection from environmental degradation from outdoor weathering to meet rigorous end user requirements.
New Developments in UV Curable Adhesive Systems
Extensive research and development has resulted in new formulations with enhanced properties. The most noteworthy are:
- USP Class VI approved compounds
 - NASA low outgassing grades
 - Nanosilica filled systems
 
Master Bond ultraviolet curable systems are presently employed in the automotive, electronic, medical, optical, electro-optical, appliance, fiber-optic and general assembly applications.
Popular UV Curable Adhesives
                        | 
                  
            UV10TKMed Biocompatible, high viscosity, UV curable compound. Optically clear. Glass transition temperature of more than 140°C. Rapid curing, no mix system. Withstands repeated sterilization. Meets USP Class VI and ISO 10993-5 cytotoxicity testing requirements. Serviceable from -60°F to +450°F.  | 
              
                        | 
                  
            UV15LV Low viscosity, high strength epoxy resin based formulation. Enhanced thermal stability. Cationic curing system. Excellent light transmission properties. Superb electrical insulation characteristics. Serviceable from -80°F to +300°F.  | 
              
                        | 
                  
            UV16 Superior chemical resistance and physical strength properties. Low shrinkage after cure. Passes NASA low outgassing tests. Excellent thermal stability. Cationic curing system. Outstanding optical clarity. Easy to apply. Low viscosity. Serviceable from -80°F to +400°F.  | 
              
                        | 
                  
            UV24TKLO Meets NASA low outgassing requirements. Excellent clarity and optical transmission properties. Outstanding chemical resistance. High dimensional stability. Moderate viscosity. Can be cured up to 1/16 of an inch and layered to higher levels. Vacuum compatibility. Serviceable from -60°F to +400°F.  | 
              
                        | 
                  
            UV10Med USP Class VI approved, optically clear adhesive. Fast curing. Resists many chemicals and sterilants. Electrically insulative. High bond strength to metals, glass, plastics such as polycarbonates, acrylics. Serviceable from -60°F to +250°F.  | 
              
			      