Formulated for specialty aviation applications, EP90FR-V is a two part, non-halogenated epoxy meeting FAR standard 14 CFR 25.853(a) for flame retardancy. It passes the vertical burn test as well as Boeing specifications BSS 7238, Revision C for smoke density and BSS 7239, Revision A for toxicity.
It features superior electrical insulation which makes it a great choice for electronic potting and sealing applications. Other product advantages are its convenient processing with a one to one mix ratio, excellent mechanical strength and long working life.