Master Bond EP21ARLV is a low viscosity epoxy capable of withstanding prolonged exposure to a wide range of acids and chemicals while maintaining excellent electrical insulation.
Two part epoxy adhesive, sealant, coating and encapsulating system featuring low viscosity and superior acid resistance
Key Features
- Convenient 2 to 1 mix ratio
- Long open time
- Good physical strength properties
- Reliable electrical insulator