142 products match
|
UV15RCL Red colored UV curable epoxy system turns clear upon exposure to UV light. Low viscosity, with superb thermal stability. Also capable of spin coating. Outstanding optical clarity. High bond strength. Serviceable from -80°F to +350°F. |
|
UV15TK Moderate viscosity single part UV curable epoxy. Cures quickly. Excellent dimensional stability. Enhanced temperature resistance. Cationic curing system. Optically clear. Volume resistivit >1014. Serviceable from -80°F to +400°F. |
|
UV15X-2 For bonding, sealing, coating, encapsulation. Fast curing no mix compound. Excellent abrasion resistant. Viscosity 3,000-9,000 cps. Shore D hardnes >70. Impressive physical strength properties. Serviceable from -80°F to 300°F. |
|
UV15X-6Med-2 UV curing system with high flexibility that is biocompatible per USP Class VI testing. Medium viscosity. Superior abrasion resistance. Non-yellowing. Reliable thermal and electrical insulator. Serviceable from -80°F to +250°F. |
|
UV15X-6Med-2LV UV curing system with high flexibility that is biocompatible per ISO 10993-5. Medium viscosity. Superior abrasion resistance. Non-yellowing. Reliable thermal and electrical insulator. Serviceable from -80°F to +250°F. |
|
UV15X-6NM-2 High flexibility and toughness. Outstanding abrasion resistance. Moderate viscosity. Resists thermal cycling and mechanical shocks. Bonds well to glass, metals, ceramics, composites and many plastics including polycarbonates, acrylics. Serviceable from -80°F to +250°F. |
|
UV15X-6NM-2BCL Low viscosity, UV curable system with superb thermal stability that turns from red to clear upon UV light exposure. Also capable of spin coating. Outstanding optical clarity. High bond strength. Serviceable from -80°F to +350°F. |
|
|
UV16 Superior chemical resistance and physical strength properties. Low shrinkage after cure. Passes NASA low outgassing tests. Excellent thermal stability. Cationic curing system. Outstanding optical clarity. Easy to apply. Low viscosity. Serviceable from -80°F to +400°F. |
|
UV18S UV curable system with superior resistance to chemicals, particularly solvents. High bond strength. Excellent light transmission properties. Electrical insulator. Low shrinkage upon cure. Exceptionally fast curing. Serviceable from -60°F to 250°F. |
|
UV19 Single component, optically clear UV curable compound. Particularly suited for laminating, bonding substrates with different thermal expansion coefficients, such as flexible soft plastic films to polyester films, metal foils. Elongatio >80%. High impact strength. Long term chemical resistance. Serviceable from -60°F to 250°F. |