UV21 Highly flexible UV curable urethane elastomer compound. Used for high performance seals, gaskets, bonding and protective coating applications. Fast curing at room temperature. Superior chemical resistance. Shore A hardness 45-55. Elongation over 260%. Viscosity 30,000-38,000 cps. Serviceable from -65°F to 250°F. |
|
UV22 UV curable, nanosilica filled system with excellent abrasion resistance. Easy to apply and fast room temperature curing upon exposure to UV light. Meets NASA low outgassing requirements. Excellent optical clarity. Superior dimensional stability. Withstands 1,000 hours 85°C/85% RH. Tg is 135°C after post curing for 30 minutes at 125-150°C. Serviceable from -80°F to +350°F. |
|
UV22DC80-1 Dual cure system with UV and heat curing mechanisms. Cures at 80°C in shadowed out areas. Nano filled, high dimensional stability and abrasion resistance. Bonds well to metals, glass, ceramics and most plastics. Serviceable from -60°F to +350°F. |
|
UV22DC80-10F Dual cure system with UV and heat curing mechanisms. Fast cures at 80°C in shadowed out areas. Nano filled, high dimensional stability and abrasion resistance. Bonds well to metals, glass, ceramics and most plastics. Minimal shrinkage upon curing. Serviceable from -60°F to +350°F. |
|
UV22DC80-1Med Dual cure system with UV and heat curing mechanisms. Cures at 80°C in shadowed out areas. Nano filled, high dimensional stability and abrasion resistance. Bonds well to metals, glass, ceramics and most plastics. Serviceable from -60°F to +350°F. |
|
UV23FLDC-80TK UV and heat curable epoxy formulation. Cures in "shadowed out" areas at temperatures as low as 80°C. Convenient no mix system. Serviceable from -80°F to +300°F. Superb electrical insulator. |
|
UV24TKLO Meets NASA low outgassing requirements. Excellent clarity and optical transmission properties. Outstanding chemical resistance. High dimensional stability. Moderate viscosity. Can be cured up to 1/16 of an inch and layered to higher levels. Vacuum compatibility. Serviceable from -60°F to +400°F. |
|
UV25 Multi-purpose, one part UV curing system for bonding, sealing, coating and encapsulation. Excellent optical clarity, superb physical properties, moderate viscosity. Ultra high glass transition temperature (Tg) over 180°C. Fast fixture times. Rapid curing. Serviceable from -60°F to +500°F. |
|
UV26 Specialty type UV curable adhesive with very fast curing time and high thermal stability. Its glass transition temperature is 160 to 170°C and its service temperature range is -60°F to +500°F. UV26 resists acids, bases, fuels, and many aggressive solvents. |
|
UV26DC Specialty type UV curable adhesive with very fast curing time and high thermal stability. Its glass transition temperature is 160 to 170°C and its service temperature range is -100°F to +400°F. UV26 resists acids, bases, fuels, and many aggressive solvents. |