EP35TDC Tough, room temperature curing epoxy paste adhesive for high temperature bonding. Serviceable from -60°F to +450-500°F. Non-drip system. Gap filling. Resistant against thermal cycling and chemical exposure. |
![]() |
EP36 One part B-staged epoxy. Flexibilized and toughened. Withstands rigorous thermal cycling and thermal shocks. Superb electrical insulation properties. Ideal for potting/encapsulation. Serviceable from -100°F to +500°F. Available in 30 gram cookies. |
![]() |
EP36AN Thermally conductive/electrically insulative B-stage epoxy potting/bonding compound. Outstanding toughness and flexibility. Resists up to 500°F. Ability to withstand thermal cycling and impact/vibration. Shore D hardness 80. Volume resistivity 1014 ohm-cm. |
![]() |
EP36AO Thermally conductive, electrically insulative B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies. Meets NASA low outgassing specifications. |
![]() |
EP36CLV One component, B-staged epoxy. Features low viscosity and excellent electrical insulation properties. Operating service temperature range -100°F to +500°F. Combines flexibility and toughness. Superior chemical resistance to water, acids, bases, fuels and oils. Elongatio >50%. |
![]() |
EP36FR Flame retardant B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies. |
![]() |
EP37-3 Resilient, optically clear, two component epoxy resin system. Long working life. Excellent electrical insulation properties. Cures accelerated by heat. Chemically resistant. Low mixed viscosity. Serviceable from -80°F to +250°F. Two to one mix ratio by weight. Withstands impact. |
![]() |
EP37-3FLF Highly flexible, low viscosity, optically clear adhesive. Resistant to severe thermal cycling and thermal shock. Bonds well to dissimilar substrates. Low exotherm system. Long working life. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume. |
![]() |
EP37-3FLFAN Highly flexible, thermally conductive/electrically insulative epoxy system. Low viscosity. Cures readily at room temperature. Long working life. One to one mix ratio by weight or volume. Serviceable from 4K to +250°F. Good physical strength and chemical resistance. |
![]() |
EP37-3FLFAO Flexible, low viscosity, thermally conductive epoxy. Meets NASA low outgassing specifications. Superb electrical insulator. Good physical strength. Chemical resistant. Long working life. Withstands 1,000 hours 85°C/85% RH. Guards against mechanical shock and vibration. Excellent flowability. Ideal for potting and casting. |