EP36CLV One Part Epoxy Compound EP36CLV

One component, B-staged epoxy. Features low viscosity and excellent electrical insulation properties. Operating service temperature range -100°F to +500°F. Combines flexibility and toughness. Superior chemical resistance to water, acids, bases, fuels and oils. Elongatio >50%.

EP36FR One Component Epoxy EP36FR

Flame retardant B-stage toughened epoxy. One part system. Ideal for potting and encapsulation. Capable of withstanding rigorous thermal shocks. Serviceable from -100°F to +500°F. Available in 30 gram cookies.

EP37-3 Two Part Epoxy System EP37-3

Resilient, optically clear, two component epoxy resin system. Long working life. Excellent electrical insulation properties. Cures accelerated by heat. Chemically resistant. Low mixed viscosity. Serviceable from -80°F to +250°F. Two to one mix ratio by weight. Withstands impact.

EP37-3FLF Two Component Epoxy System EP37-3FLF

Highly flexible, low viscosity, optically clear adhesive. Resistant to severe thermal cycling and thermal shock. Bonds well to dissimilar substrates. Low exotherm system. Long working life. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume.

EP37-3FLFAN Two Part Epoxy System EP37-3FLFAN

Highly flexible, thermally conductive/electrically insulative epoxy system. Low viscosity. Cures readily at room temperature. Long working life. One to one mix ratio by weight or volume. Serviceable from 4K to +250°F. Good physical strength and chemical resistance.

EP37-3FLFAO Two Part Epoxy EP37-3FLFAO

Flexible, low viscosity, thermally conductive epoxy. Meets NASA low outgassing specifications. Superb electrical insulator. Good physical strength. Chemical resistant. Long working life. Withstands 1,000 hours 85°C/85% RH. Guards against mechanical shock and vibration. Excellent flowability. Ideal for potting and casting.

Two Part Epoxy EP37-3FLFAOND EP37-3FLFAOND

Highly flexible, low viscosity adhesive. Resistant to severe thermal cycling and thermal shock. Bonds well to dissimilar substrates. Low exotherm system. Long working life. Superior electrical insulation properties. Service temperature range from 4K to +250°F. One to one mix ratio by weight or volume.

EP37-3FLSP Two Component Epoxy EP37-3FLSP

Highly flexible. Low viscosity. Optically clear. Serviceable from 4K to +200°F. Superior dimensional stability. Long working life and low exotherm during curing. Ideal for large volume potting and casting. Excellent impact resistant.

EP37-3LV Two Part Epoxy System EP37-3LV

Clear, two component epoxy system has long pot life. Convenient one to one mix ratio. High bond strength. Superb chemical resistance properties. Used in bonding, sealing, potting and filament winding applications. Low viscosity compound. Exceptionally low exotherm. Cures rigid. Service operating temperature range from -60°F to +250°F.

EP38 Two Component Epoxy EP38

Electrically insulative compound. Excellent flowability. High flexibility. Superior tensile and compressive strength. Cures quickly. Outstanding optical clarity. Protect against boiling water. Short tack free time. Low shrinkage upon cure. Easy to apply by roller, brush, spray equipment. Serviceable from -60°F to +250°F.