Master Bond Product Search

557 products match

EP46CA Two Part Epoxy EP46CA

Oven curing. Two component epoxy for bonding/sealing. Long pot life. Serviceable from -100°F to +600°F. T > 240°C. High bond strength. Outstanding electrical insulation properties. Robust chemical resistance.

EP46CA-1 Two Part Epoxy EP46CA-1

Serviceable from -100°F to +600°F. Tg>240°C. Oven curing. Used for structural bonding. High bond strength to similar/dissimilar surfaces. Withstands thermal cycling and chemical exposure. Electrical insulator. Long working life.

EP46HT Two Part Epoxy EP46HT

Heat resistant epoxy adhesive/sealant. Exhibits exceptional mechanical strength. Low viscosity system. Long pot life. Cures at elevated temperatures. Long term high temperature structural strength retention. Serviceable from -80°F to +500°F. Outstanding chemical resistance. Used in filament windings and with composite structures made from glass, polymide and graphic fiber.

EP46HT-1 Two Part Epoxy Compound EP46HT-1

Oven curing two part epoxy system. Resists from -100°F to +600°F. Tg of 230-240°C . Superb choice as matrix resin for fiber reinforced heat resistant composite structures. Exceptional strength properties. Robust chemical resistance. Long working life after mixing.

EP46HT-1AO Two Part Epoxy Compound EP46HT-1AO

Thermally conductive/electrically insulative heat resistant epoxy compound. Requires oven curing. Meets NASA low outgassing specifications. Meets MIL-STD-883J Section 3.5.2 for thermal stability. Excellent dimensional stability. Withstands 1,000 hours 85°C/85% RH. Serviceable from -100°F to +550°F. Tg 215-220°C.

EP46HT-1ND2 Two Part Epoxy System EP46HT-1ND-2

Heat resistant epoxy paste adhesive. Serviceable from -100°F to +600°F. Requires oven curing. Will not flow during processing. Superior electrical insulation and chemical resistant properties. Excellent mechanical strength.

EP46HT-2 Two Part Epoxy EP46HT-2

Serviceable from -100°F to +500°F. Tg 155-165°C. Superior durability. Heat curing, two component epoxy compound. Resists thermal cycling. Withstands 1,000 hours 85°C/85% RH. Good electrical insulator. Ability to protect against hostile chemical exposure.

EP46HT-2AO Black Two Part Epoxy EP46HT-2AO Black

Thermally conductive/electrically insulative. Passes NASA low outgassing tests. Serviceable from -100°F to +500°F. Tg 200-210°C. Remarkable dimensional stability. Impressive mechanical strength properties.

EP46HT-2Med Two Component Epoxy EP46HT-2Med

USP Class IV approved, heat resistant epoxy adhesive. Glass transition temperature in excess of 220°C. Withstands repeated exposure to autoclaving, radiation and chemical sterilants. High bond strength. Superior durability. Serviceable from -100°F to +500°F. Electrically insulative SUitable for potting.

EP46HT-2ND2 Two Part Epoxy Compound EP46HT-2ND2

Two part non-drip epoxy paste. Resists long term exposure from -100°F to +550°F. Superior peel strength. Protects against exposure to oils, fuels, hydrocarbons, acids, bases, solvents. Withstands thermal cycling and shock.