Supreme 45HT-3 Toughened, thermally stable, two component epoxy adhesive, sealant, coating. Excellent compressive strength. Abrasion resistant. Withstands exposure to acids, bases, solvents, fuels, oils, water. Electrical insulator. Service temperature range -100°F to +550°F. |
![]() |
Supreme 45HTAO Toughened, thermally conductive epoxy compound. Superb electrical insulator. Resists -80°F to +500°F. High strength properties. Two part system. Oven curing. Long-term durability. |
![]() |
Supreme 45HTND Toughened, non-drip epoxy paste for bonding, sealing, coating. Serviceable from -100°F to +450°F. Two component system has long working life. Heat curing. High peel/shear strength properties. Withstands rigorous thermal cycling. |
![]() |
Supreme 45HTND-2 Paste viscosity. Will not flow when cured. Gap filling. Serviceable from -100°F to +450°F. High peel and shear strength properties. Two part system. Long pot life. Good thermal cycling capabilities. Excellent electrical insulator. |
![]() |
Supreme 45HTND-2LO Black Toughened, two component, non-drip epoxy paste. Service temperature range -100°F to +450°F. Long working life. Gap filling. Meets NASA low outgassing specifications. Withstands 1,000 hours 85°C/85% RH. Superior electrical insulator. Heat curing. |
![]() |
Supreme 45HTQ Two component, toughened, quartz filled epoxy with exceptional abrasion resistance. Heat curing system. Long working life after mixing. High compressive strength. Superb dimensional stability. Serviceable from -60°F to +450°F. Withstands exposure to petrochemicals acids, bases, solvents. Good strength retention at elevated temperatures. Successfully tested for 1,000 at 85°C/85% RH. |
![]() |
Supreme 45HTQ-4 Toughened, two component silicon carbide filled epoxy. Heat curable. Exceptional abrasion and chemical resistance. Serviceable from -100°F to +450°F. Can withstand high compressive loads and rigorous thermal cycling. Good strength retention at elevated temperatures. |
![]() |
Supreme 46HT-1AO Toughened epoxy system, resists thermal cycling. Serviceable from -100°F to +500°F. Exceptionally long working life. Thermally conductive, electrically insulative. |
![]() |
Supreme 46HT-2 High strength epoxy adhesive. Outstanding toughness and durability. Serviceable from -100°F to +500°F. Withstand mechanical shocks and rigorous thermal cycling. Excellent peel strength. Cures at elevated temperature. |
![]() |
Supreme 46HT-2ND2 Two component, non-drip, toughened, heat resistant epoxy adhesive. Superior durability and bond strength. Withstands chemical exposure. Paste consistency. Gap filling. Serviceable from -100°F to +500°F. Successfully tested for 1,000 hours 85°C/85% RH. Outstanding thermal cycling capabilities. |