MasterSil 151 Optically clear, addition curing potting, encapsulation, sealing compound. Low shrinkage upon cure. Resists up to +400°F [+204°C]. Shore A hardness 50-60. Highly resistant to water. Long pot life. |
|
MasterSil 151Med Black ISO 10993-5 approved for non-cytotoxicity. Silicone system, Addition cured. Optically opaque. Offers ambient or elevated temperature cures. Excellent for potting and encapsulation applications. Low shrinkage upon cure. Resists gamma radiation, EtO and various chemical sterilants. Serviceable from -65°F to +400°F. |
|
MasterSil 151Med Medical grade, USP Class VI approved silicone. Addition type cure system. Optically clear. Low outgassing. Offers ambient or elevated temperature cures. Excellent for potting and encapsulation applications. Low shrinkage upon cure. Resists gamma radiation, EtO and various chemical sterilants. Serviceable from -65°F to +400°F. |
|
MasterSil 152 Low viscosity, optically clear condensation curing system. Superb flexibility and electrical insulation properties. Long pot life. Will cure in section >1 inch. Low exotherm. Elongation 150-180%. Serviceable from -65°F to +400°F. |
|
MasterSil 157 Two component low viscosity silicone system. Ideal for potting and encapsulation. Does not require air for curing. Low exotherm; very long pot life. Enhanced low temperature serviceability. Service temperature range of -175°F to +500°F. Superior electrical insulator. |
|
MasterSil 170 Gel Two part, low viscosity silicone gel for sealing, potting and encapsulating applications. Outstanding flexibility. Superior electrical insulation properties. Exceptional optical clarity. Serviceable from -67°F to +392°F. |
|
MasterSil 323 Two part silicone paste for bonding, sealing and encapsulating applications. Optically clear in thin sections. Outstanding flexibility. Contains no solvents or diluents. Low to moderate viscosity. Low dielectric constant. Addition cured, no by-products released during cure. Serviceable from -65°F to +400°F. |
|
MasterSil 323Med Two part silicone paste for bonding, sealing and encapsulating applications. Optically clear in thin sections. Outstanding flexibility. Contains no solvents or diluents. Low to moderate viscosity. Low dielectric constant. Addition cured, no by-products released during cure. Serviceable from -65°F to +400°F. |
|
MasterSil 415 Optically clear, room temperature curing, no mix acetoxy type system. Good bond strength and outstanding elasticity. Serviceable from -185°F to 400°F. |
|
MasterSil 920-LO RTV silicone for sealing, coating and small encapsulation. NASA low outgassing approved. Superb optical clarity. Good flow properties. Non-corrosive. Soft durometer facilitates usage with sensitive components. Excellent electrical insulator. Withstands thermal cycling. |