EP21LP Gray Product Information | MasterBond.com

EP21LP Gray Two Component Epoxy

Key Features

  • Moderate viscosity
  • Electrically insulative
  • Room temperature curing
  • One to one mix ratio — rigid to flexible cure
  • Shore D hardness 70-80
  • Dimensionally stable