EP21NDFG Product Information | MasterBond.com

Two component epoxy compound for high performance applications

EP21NDFG Two Component Epoxy

Key Features

  • Meets FDA Section 175.105 requirements
  • One to one mix ratio
  • Room temperature curing
  • Non-drip paste
  • For bonding, sealing and coating
  • Chemical resistant
Back to Top