One component epoxy system for bonding, sealing and coating
Key Features
- No mixing and convenient processing
 - Toughened system
 - Wide service temperature range of -80°F to +350°F
 - Superb thermal and electrical insulator
 
Product Description
Master Bond EP3HTFL is a one part system that offers easy processing along with excellent physical strength and adhesive properties. It is a true one part system, not premixed and frozen, and can be stored either at room temperature or in a refrigerator. The system does, however, require oven curing with a minimum temperature of 250°F. As noted in the table, it cures rapidly at 250°F and even more quickly at 300°F. In essence, it has an unlimited working life at room temperature. Also, it is a toughened or slightly flexibilized system. This allows the system to withstand rigorous thermal cycling and shock.
EP3HTFL bonds well to a wide variety of substrates including glass, metals, composites, ceramics and many plastics. It has good chemical resistance to water, oils, fuels and hydraulic fluids. EP3HTFL is a good thermal and electrical insulator. The color of EP3HTFL is tan to brown. Its service temperature range is -80°F to +350°F. This epoxy system is useful in aerospace, electronic, electrical and specialty OEM applications, particularly when bonding dissimilar substrates that are subjected to thermal cycling and shock.
Product Advantages
- Single component system; no mixing required
 - Unlimited working life at room temperature
 - Easy to apply
 - Fast curing
 - Good bond strength to many substrates
 - Capable of withstanding thermal cycling
 