EP41S-6 Product Information | MasterBond.com

Two component epoxy system that meets UL 1203 for Explosion-Proof and Dust-Ignition-Proof Electrical Equipment for Use in Hazardous (Classified) Locations

Key Features

  • Convenient handling
  • Good flow properties
  • Black color
  • High temperature resistant