Two component, graphite conductive epoxy system for bonding, sealing, coating

Key Features

  • Cures at room temperature
  • Non magnetic; graphite filled
  • Good electrical conductivity
  • Withstands 1,000 hours 85°C/85% RH

Product Description

Master Bond EP75-1 is a two component, graphite filled, electrically conductive epoxy for high performance bonding, sealing and coating. The mix ratio of the EP75-1 system is 100 to 15 by weight. It can cure at room temperature or more rapidly at elevated temperatures. The optimum cure schedule is overnight at 75°F followed by 1-2 hours at 150-200°F. The volume resistivity of EP75-1 is 50-100 ohm-cm placing it in the realm of applications involving static dissipation and for EMI/RFI shielding purposes. The graphite filler confers non-magnetic properties as well as a modicum of lubricity to the system. In fact, EP75-1 is a material of choice when the requirement is for a non-metallic electrically conductive epoxy.

EP75-1 contains no solvents and has a paste-like consistency after mixing. It bonds well to a wide variety of substrates including metals, composites, ceramics, glass and many rubbers and plastics. It has reputable lap shear strength of over 1,400 psi along with worthy dimensional stability. It has good chemical resistance to water, oils, acids and bases. Its service temperature range is 4K to +250°F. It can be used for electronic, aerospace, semiconductor, medical, fiber-optic, specialty OEM and related applications where a cost effective system for dissipating static electricity or EMI/RFI shielding, among the other properties mentioned above, might be needed.

Product Advantages

  • Versatile cure schedules
  • Well suited for shielding and static dissipation
  • Non-magnetic
  • Good lubricity
  • Outstanding dimensional stability
  • Cryogenically serviceable
  • Meets NASA low outgassing specifications

Industrial Certifications


ASTM E595 Compliant

1,000 Hours at 85°C/85% RH

Meets EU Directive 2015/863

Packaging


Cans

Jars

EP75-1 is available is various sizes and units to accommodate customer's needs.

Case Studies

Request Information