Two component high strength epoxy system complying with FAR standard 14 CFR 25.853(a) for flame retardancy

Key Features

  • Tested as per Amendment 25-116 and Part 25 Appendix F
  • Passes horizontal burn test
  • Two to one mix ratio
  • For bonding, sealing and coating

Product Description

Master Bond EP90FR-H is a two component flame retardant epoxy system for bonding, sealing, coating and potting. It has been tested to the standards mentioned above and passes the difficult horizontal burn test specification. This moderate viscosity system has excellent strength properties and can be considered for use in specialized applications especially in aircraft and related assemblies. Some potential uses include baggage equipment areas, aircraft windows and lighting assemblies, among others. Additionally, it should be noted that EP90FR-H is a non-halogenated type system, which is highly desirable for handling and environmental issues.

EP90FR-H has an easy to use, forgiving, two to one mix ratio by weight. This system has a moderately long open time with the recommended curing for optimizing properties being overnight at room temperature followed by 2-3 hours at 150-200°F. It is a very good electrical insulator, and can be used in electronics for bonding, sealing and coating. It bonds well to a variety of substrates including metals, composites, glass, ceramic and many plastics. The system is color coded; Part A is gray, Part B is white and when mixed it becomes a noticeably lighter gray. It has good chemical resistance to water, fuels and oils. The service temperature range is -60°F to +250°F. EP90FR-H is a specialty product primarily for aviation and avionic applications where the arduous prerequisites of the horizontal burn test are specified.

Product Advantages

  • Easy to use, forgiving 1:1 mix ratio by weight
  • Superb electrical insulator
  • Superior adhesion to a wide variety of substrates
  • High dimensional stability
  • Exceptionally low shrinkage upon curing
  • Meets the stringent horizontal burn test portion of the FAR standard 14 CFR 25.853(a) for flame retardancy
  • Non halogen filler

Industrial Certifications


FAR 25.853(a) for Flame Retardancy

Packaging


Cans

Pails

Premixed & Frozen Syringe

EP90FR-H is available is various sizes and units to accommodate customer's needs.