EP45HTQ Product Description

EP45HTQ Two Component Epoxy

Two Component Quartz Filled Heat Resistant Epoxy Compound for High Performance Structural Bonding, and Casting.

EP46HT Product Information

EP46HT Two Part Epoxy

Two Component High Performance Epoxy Resin System for Heat Resistant Structural Bonding, Sealing And Castings.

EP46HT-1 Product Information

EP46HT-1 Two Part Epoxy Compound

Two Component Heat Resistant Epoxy System for High Performance Structural Bonding and Sealing, Featuring a Glass Transition Temperature in Excess of 235°C.

EP46HT-2 Product Information

EP46HT-2 Two Part Epoxy

Two Component, Heat Resistant, Epoxy System for High Performance Bonding, Sealing and Casting. Features a Glass Transition Temperature in Excess of 220°C; Requires Elevated Temperature Curing at 250°F or Above.

EP46HT-2AO Black Product Information

EP46HT-2AO Black Two Part Epoxy

Two Component, Thermally Conductive, Electrically Insulating Epoxy for High Performance Bonding, Sealing and Encapsulation. Features a Glass Transition Temperature in Excess of 200°C; Requires Elevated Temperature Curing at 250°F or Above. Meets NASA Low Outgassing.

EP46HT-2Med Product Information

EP46HT-2Med Two Component Epoxy

Two Component Heat Resistant Epoxy System for High Performance Structural Bonding and Casting Featuring a Glass Transition Temperature in Excess of 220°C Suitable for Repeated Autoclaving, Radiation and Chemical Sterilants Meets USP Class VI Requirements

EP51HT Product Description

EP51HT Two Part Epoxy

Two Component, Room Temperature Curing Epoxy Adhesive Featuring Superior and Cost Effective Bonding Performance with Exceptionally Fast Cures for Service from 4K to 400°F.

EP62-1 Product Information

EP62-1 Two Part Epoxy System

Two Component Epoxy System Features a Very Long Pot Life at Ambient Temperatures Combined with Rapid Cures Chemical and High Temperature Resistance

EP62-1Med Product Information

EP62-1Med Two Component Epoxy System

Two Component Epoxy Resin System Features a Very Long Pot Life at Ambient Temperatures Combined with Rapid Cures at Moderately Elevated Temperatures and Chemical and High Temperature Resistance.

Meets USP Class VI Requirements.

EP65HT Product Information

EP65HT Two Component Epoxy

Two Component Epoxy System Featuring the Unique Combination of Very Fast Setting and Curing Along with High Temperature Resistance.