EP21TDC-2ND Product Information

EP21TDC-2ND Two Part Epoxy

Two Component Epoxy System with Outstanding Flexibility and Peel Strength for High Performance Bonding, Sealing, Coating and Encapsulation. Serviceable at Cryogenic Temperatures.

Supreme 42HT-2ND Product Information

Supreme 42HT-2ND Two Part Epoxy

Toughened, Two Component Epoxy Adhesive/Sealant Featuring High Temperature and Chemical Resistance; Superior Thermal Cycling Capabilities.

MB350 Product Information

MB350 Alkoxyethyl Cyanoacrylate System

High viscosity ethyl cyanoacrylate with excellent performance profile

Supreme 3HTND-2DA Product Information

Supreme 3HTND-2DA One Part Epoxy

One component, toughened, electrically insulating epoxy for die attach applications

Supreme 45HTND-2LO Black Product Information

Supreme 45HTND-2LO Black Two Part Epoxy

Toughened, two component epoxy system featuring high temperature resistance and NASA low outgassing

EP41S-F Product Information

EP41S-F Two Part Epoxy System

Versatile, two part epoxy system for bonding, sealing, coating and encapsulating

EP13SPND-2 Product Information

EP13SPND-2 One Part Heat Cure Epoxy

One component, heat curing epoxy for structural bonding applications