UV24TKLO Product Information

UV24TKLO One Part UV Curable System

One Component, Moderate Viscosity, UV-Curable System for Bonding, Sealing and Encapsulation Featuring Superior Chemical Resistance. Meets NASA Low Outgassing Requirements.

X-5 Product Description

Elastomer Based, One Component Adhesive

High Performance, Elastomer-Based, One-Component Adhesive for Fast & Durable Bonding and Sealing

X-5HT Product Description

High Performance High Temperature, Structural One-Component Adhesive System For Fast, Durable Bonding and Sealing Up To 500°F Service

X5TC Product Information

X5TC One Part Elastomeric System

Thermally Conductive, Elastomer Based, One-Component Adhesive For High Performance Bonding and Sealing